Aluminum I-Beams
Directory
|
Career
|
News
|
Standards
|
Industrial
|
SpecSearch®
Design Home
Standard Beams
Steel W Type I-Beam
Steel S Type I-Beam
Steel Channels
Steel Angles
Alumimun I-Beams
Aluminum Channels
Common Beams
Square I-Beam
Tapered I-Beam
Uneven I-Beam
General Shape
Square Channel
Tapered Channel
Square L Beam
Rectangular L Beam
Square T Beam
Semi-tapered T Beam
Tapered T Beam
Rectangular Cross
Applications
Beam Bending
Bibliography
Login
FREE Publications
Design News
NASA Tech Briefs
Waste Management
Renewable Energy
Chemical Engineering
Filtration+Separation
Processing Magazine
Design-2-Part
more
...
ASME Membership
25% Off
Exclusive partnership
offers for efunda users.
Home
Membership
Magazines
Forum
Search Member
Calculators
Materials
Design
Processes
Units
Formulas
Math
Aluminum I-Beams
The I-Beams are identified by:
DEPTH (inches) × WEIGHT PER UNIT LENGTH (pound force per foot)
For Example:
12 × 14.292
is an I-Beam 12 inches deep and weighing 14.292 lbs/ft.
Check all the I-Beams you would like to see properties for and then click GET.
12 × ___
10 × ___
9 × ___
8 × ___
7 × ___
12.00 × 14.292
10.00 × 10.286
9.00 × 8.361
8.00 × 7.023
7.00 × 5.800
12.00 × 11.672
10.00 × 8.646
8.00 × 6.181
6.00 × 4.692
6 × ___
5 × ___
4 × ___
3 × ___
6.00 × 4.030
5.00 × 3.700
4.00 × 2.793
3.00 × 2.030
4.00 × 2.311
3.00 × 1.637
ALL