eFunda: Properties of Alloy Steel Alloy Steel AA 3004
engineering fundamentals Alloy Steel Alloy Steel AA 3004
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AA 3004
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  97.8 
Mn  1.2 
Mg  1.0 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.6-2.8 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 215  25  H32  more
Yield Strength (Mpa) 170 
Elongation (%) 10 
Reduction in Area (%)  
Hardness (HB500) 52  25  H32 more
Shear Strength (MPa) 115  25  H32  more
Fatigue Strength (MPa) 105  25  H32  more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Conductivity (W/m-K) 162  25  O (all) 

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 41  25  O(all) 