eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel AA 4043
Alloy Steel Alloy Steel Alloy Steel AA 4043
Directory
|
Career
|
News
|
Standards
|
Industrial
|
SpecSearch®
Keywords
AISI (US)
UNS (US)
SAE (US)
ASTM (US)
AMS (US)
ASME (US)
MIL (US)
FED (US)
DIN (DEU)
JIS (JPN)
AFNOR(FR)
B.S. (UK)
SS (SWE)
UNI (ITA)
Aluminum
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
*
For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Resources
Bibliography
Trade Publications
Photonics Spectra
Pipeline and Gas Tech
Laser Focus World
World Pumps
Equipment World
Metal Finishing
more
Login
Home
Membership
Store
Forum
Search Member
Calculators
Materials
Design
Processes
Units
Formulas
Math
AA 4043
Conditions
Tensile Properties
T
(°C)
Treatment
25
H18
Tensile Strength
(MPa)
285
Yield Strength
(MPa)
270
Elongation
(%)
0.5
Reduction in Area
(%)
25
O
Tensile Strength
(MPa)
145
Yield Strength
(MPa)
69
Elongation
(%)
22
Reduction in Area
(%)
Glossary
Materials » Alloys » Aluminum Alloy » Wrought » AA 5056
Materials » Alloys » Steel » Alloy Steel » ASTM A517 Grade C
Materials » Alloys » Steel » Alloy Steel » AISI 5132
Materials » Alloys » Steel » Alloy Steel » SAE 950X
Materials » Alloys » Steel » Alloy Steel » ASTM A517 Grade P
Materials » Alloys » Steel » Alloy Steel » ASTM A514 Type H
Materials » Alloys » Copper Alloy » Wire » AWG-40
Materials » Alloys » Steel » Carbon Steel » AISI 1572
Materials » Alloys » Steel » Alloy Steel » ASTM A441
Materials » Alloys » Steel » Alloy Steel » AISI 8640
Home
Membership
About Us
Privacy
Disclaimer
Contact
Advertise
Copyright © 2009 eFunda, Inc.