eFunda: Properties of Alloy Steel Alloy Steel AISI 8620H
Alloy Steel Alloy Steel AISI 8620H
Directory
|
Career
|
News
|
Standards
|
Industrial
|
SpecSearch®
Keywords
AISI (US)
UNS (US)
SAE (US)
ASTM (US)
AMS (US)
ASME (US)
MIL (US)
FED (US)
DIN (DEU)
JIS (JPN)
AFNOR(FR)
B.S. (UK)
SS (SWE)
UNI (ITA)
Aluminum
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
*
For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Resources
Bibliography
Trade Publications
Adhesives & Sealants
Paint & Coatings
Ceramic Industry
Laser Focus World
NASA Tech Briefs
World Pumps
more
Login
Home
Membership
Store
Forum
Search Member
Calculators
Materials
Design
Processes
Units
Formulas
Math
AISI 8620H
Conditions
Tensile Properties
T
(°C)
Treatment
25
annealed at 870°C
Tensile Strength
(MPa)
650
Yield Strength
(MPa)
385
Elongation
(%)
31.3
Reduction in Area
(%)
62
25
normalized at 915°C
Tensile Strength
(MPa)
635
Yield Strength
(MPa)
360
Elongation
(%)
26.3
Reduction in Area
(%)
60
Glossary
Materials » Alloys » Copper Alloy » Wire » AWG-30
Beams » Simply Supported » Uniformly Distributed Load » Single Span » Aluminum I Beam » 4.00 × 2.793
Materials » Alloys » Steel » Alloy Steel » AISI 8640
Materials » Alloys » Steel » Alloy Steel » ASTM A204 Grade C
Materials » Alloys » Steel » Alloy Steel » SAE 950B
Materials » Alloys » Steel » Alloy Steel » AISI 8625
Materials » Alloys » Steel » Alloy Steel » SAE 950X
Materials » Alloys » Steel » Alloy Steel » ASTM A514 Type B
Materials » Alloys » Copper Alloy » Wire » AWG-2
Materials » Alloys » Steel » Alloy Steel » AISI 8637H
Home
Membership
About Us
Privacy
Disclaimer
Contact
Advertise
Copyright © 2009 eFunda, Inc.