eFunda: Properties of Alloy Steel AISI Type 436
engineering fundamentals Alloy Steel AISI Type 436
Directory | Career | News | Industrial
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI Type 436
Category Steel
Class Stainless steel
Type Ferritic standard
Common Names Chromium steel
Designations  United States: SAE 51436 , SAE J405 (51436) , UNS S43600

Composition

ElementWeight %
C  0.12 
Mn  1.00 
Si  1.00 
Cr  16.0-18.0 
P  0.04 
S  0.03 
Mo  0.75-1.25 
Nb+Ta  0.6 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 200 25  
Tensile Strength (Mpa) 530  25  annealed (sheet, strip) 
Yield Strength (Mpa) 365 
Elongation (%) 23 
Reduction in Area (%)  
Hardness (HRB) 83 (max)  25  annealed (sheet, strip) 

Thermal Properties

Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 9.3  0-100  
Thermal Conductivity (W/m-K) 23.9  100 more  
Specific Heat (J/kg-K) 460  0-100   

Electric Properties

Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 600  25   