eFunda: Properties of Carbon Steel AISI 1023
engineering fundamentals Carbon Steel AISI 1023
Directory | Career | News | Industrial
Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI 1023
Category Steel
Class Carbon steel
Type Standard
Designations  France: AFNOR XC 18 S , AFNOR XC 25
Germany: DIN 1.1151
Japan: JIS S 20 CK , JIS S 22 C , JIS S2OC
United States: ASTM A29 , ASTM A510 , ASTM A575 , ASTM A576 , ASTM A659 , SAE J403 , SAE J412 , SAE J414 , UNS G10230

Composition

ElementWeight %
C  0.20-0.25 
Mn  0.30-0.60 
P  0.04 (max) 
S  0.05 (max) 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.858 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 425  25  cold drawn (round bar (19-32 mm)) more
Yield Strength (Mpa) 360 
Elongation (%) 15 
Reduction in Area (%) 40 
Hardness (HB) 121  25  cold drawn (round bar (19-32 mm)) more

Thermal Properties

Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 12.1  20-100 more  
Thermal Conductivity (W/m-K) 51.2  100 more  
Specific Heat (J/kg-K) 486  50-100 more  

Electric Properties

Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 169  20 more  