eFunda: Properties of Carbon Steel AISI 15B41H
engineering fundamentals Carbon Steel AISI 15B41H
Directory | Career | News | Industrial
Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI 15B41H
Category Steel
Class Carbon steel
Type H-steel
Common Names Boron steel
Designations United States: UNS H15411

Composition

ElementWeight %
C  0.35-0.45 
Mn  1.25-1.75 
P  0.04 (max) 
S  0.05 (max) 
Si  0.15-0.30 
B  0.0005-0.003 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  