eFunda: Properties of Carbon Steel ASTM A570 Grade 30
engineering fundamentals Carbon Steel ASTM A570 Grade 30
Directory | Career | News | Industrial
Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
ASTM A570 Grade 30
Category Steel
Class Carbon steel

Composition

ElementWeight %
C  0.25 
Mn  0.90 
P  0.04 
S  0.05 
Cu  0.20 (min) 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 340  25   
Yield Strength (Mpa) 205 
Elongation (%) 17-19 
Reduction in Area (%)  