ASTM A611 Grade C |
 |
|
| Category | Steel |
| Class | Carbon steel |
| Composition |
 |
|
| Element | Weight % |
| C |
0.20 |
| Mn |
0.60 |
| P |
0.04 |
| S |
0.04 |
| Cu |
0.20 (min) |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.7-8.03
|
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
| Tensile Strength (Mpa) |
330 |
25 |
|
| Yield Strength (Mpa) |
230 |
| Elongation (%) |
22 |
| Reduction in Area (%) |
|
|