AWG-5
Category Copper Alloy
Class Wire
Type Round copper wire
Designations United States: ASTM B1, ASTM B3, ASTM B258

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  