UNS C65500 |
 |
|
| Category | Copper Alloy |
| Class | Wrought |
| Type | High-silicon bronze, A |
| Designations | United States: UNS C65500 |
| Composition |
 |
|
| Element | Weight % |
| Cu |
97.0 |
| Si |
3.0 |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
8.8-8.94
|
25 |
|
| Poisson's Ratio |
0.34 |
25 |
|
| Elastic Modulus (GPa) |
117
|
25 |
|
| Tensile Strength (Mpa) |
386-1000
|
25 |
(flat products, rod, wire, tube) more |
| Yield Strength (Mpa) |
145-483
|
| Elongation (%) |
63 |
| Reduction in Area (%) |
|
| Note: Elongation is measured in 3 inches. |
|