AISI 5015 |
 |
|
| Category | Steel |
| Class | Alloy steel |
| Type | Standard |
| Common Names | Chromium steel |
| Designations | United States: UNS G50150 |
| Composition |
 |
|
| Element | Weight % |
| C |
0.12-0.17 |
| Mn |
0.30-0.50 |
| P |
0.035 (max) |
| S |
0.04 (max) |
| Si |
0.15-0.30 |
| Cr |
0.30-0.50 |
| B |
0.0005-0.003 |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.7-8.03
|
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
|