eFunda: Properties of Stainless Steel AISI 5155H
engineering fundamentals Stainless Steel AISI 5155H
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI 5155H
Category Steel
Class Alloy steel
Type H-steel
Common Names Chromium steel
Designations  France: AFNOR 55 C 3
Germany: DIN 1.7176
United States: ASTM A304 , SAE J1268 , UNS H51550

Composition
ElementWeight %
C  0.50-0.60 
Mn  0.60-1.00 
Cr  0.60-1.00 
P  0.035 
S  0.040 
Si  0.15-0.30 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  