eFunda: Properties of Stainless Steel AISI Type 410
engineering fundamentals Stainless Steel AISI Type 410
Directory | Career | News | Standards | Industrial | SpecSearch®
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI Type 410
Category Steel
Class Stainless steel
Type Martensitic standard
Common Names Chromium steel
Designations  France: AFNOR Z 10 C 13 , AFNOR Z 10 C 14 , AFNOR Z 12 C 13
Germany: DIN 1.4006
Italy: UNI X 12Cr 13
Japan: JIS SUS 410
Sweden: SS 2302
United Kingdom: B.S. 410 S 21 , B.S. ANC 1 Grade A , B.S. En. 56 A
United States: AMS 5504 , AMS 5591 , AMS 5613 , AMS 5776 , AMS 5821 , ASME SA194 (Type 6) , ASME SA240 , ASME SA268 , ASME SA479 , ASTM A176 , ASTM A193 , ASTM A194 , ASTM A240 , ASTM A276 , ASTM A314 , ASTM A473 , ASTM A479 , ASTM A493 , ASTM A511 , ASTM A580 , FED QQ-S-763 , FED QQ-W-423 , MIL SPEC MJL-S-862 , SAE 51410 , SAE J405 (51410) , SAE J412 (51410) , UNS S41000

Composition

ElementWeight %
C  0.15 
Mn  1.00 
Si  1.00 
Cr  11.5-13.0 
P  0.04 
S  0.03 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 200 25  
Tensile Strength (Mpa) 485  25  annealed, hot finished (wire) more
Yield Strength (Mpa) 275 
Elongation (%) 20 
Reduction in Area (%) 45 
Hardness (HRB) 95 (max)  25  annealed (plate, sheet, strip) 

Thermal Properties

Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 9.9  0-100 more  
Thermal Conductivity (W/m-K) 24.9  100 more  
Specific Heat (J/kg-K) 460  0-100   

Electric Properties

Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 570  25   