eFunda: Properties of Stainless Steel Stainless Steel Stainless Steel AISI Type 416
engineering fundamentals Stainless Steel Stainless Steel Stainless Steel AISI Type 416
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI Type 416
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (wire)  Tensile Strength (MPa) 585-860
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  
25 hard temper (wire)  Tensile Strength (MPa) 965-1210
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  
25 intermediate temper (wire)  Tensile Strength (MPa) 795-1000
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  