eFunda: Properties of Stainless Steel Stainless Steel Stainless Steel AISI Type 430F
engineering fundamentals Stainless Steel Stainless Steel Stainless Steel AISI Type 430F
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI Type 430F
Category Steel
Class Stainless steel
Type Ferritic standard
Common Names Chromium steel
Designations  France: AFNOR Z 10 CF 17
Germany: DIN 1.4104
Italy: UNI x 10 CrS 17
Japan: JIS SUS 430
Sweden: SS 2383
United States: ASTM A314 , ASTM A473 , ASTM A581 , ASTM A582 , MIL SPEC MIL-S-862 , SAE 51430F , SAE J405 (51430F) , UNS S43020

Composition
ElementWeight %
C  0.12 
Mn  1.25 
Si  1.00 
Cr  16.0-18.0 
P  0.06 
S  0.15 (min) 
Mo(optional)  0.6 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 200 25  
Tensile Strength (Mpa) 722.5  25  annealed (wire) 
Yield Strength (Mpa) 105 
Elongation (%)  
Reduction in Area (%)  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 10.4  0-100 more  
Thermal Conductivity (W/m-K) 26.1  100 more  
Specific Heat (J/kg-K) 460  0-100   

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 600  25   