eFunda Polymers: Properties of Fluoroplastics {THV-400}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Fluoroplastics
 
List of Suppliers
State: THV-400
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Tensile Strength (MPa)   24 at break   D638
Elongation at break (%)   500     D638
Hardness   53  Shore   D638

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  1.97   D792

 Processing Properties Conditions
Type ASTM
Melting Temperature (ºC)  150  Tm, crystalline  
Processing Temperature (ºC)  244  extrusion  