eFunda Polymers: Properties of Polyester / alkyd, thermoset {alkyd, mineral filled, molding compounds, granular and putty}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Polyester / alkyd, thermoset
 
List of Suppliers
State: alkyd
Additives: mineral filled
Application: molding compounds, granular and putty
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Elastic Modulus (MPa)   3450 - 20700  tensile   D638
 13800 - 20700  compressive   D638
Flexural Modulus (MPa)  13800   23 ºC   D790
Tensile Strength (MPa)   21 - 63 at break   D638
Compressive Strength (MPa)
at yield or break
  83 - 263     D695
Flexural Strength (MPa)
at yield or break
  42 - 118     D790
Hardness   98  Rockwell E   D638
Izod Impact (J/cm of notch)
1/8" thick specimen unless noted
  0.2 - 0.3     D256A

 Thermal Properties Conditions
Pressure State ASTM
Coef of Thermal Expansion (10-6/ºC)   20 - 50     D696
Deflection Temperature (ºC)  177 - 260   1.82 MPa   D648
Thermal Conductivity (W/m-ºC)  0.502 - 1.045     C177

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  1.6 - 2.3   D792
Water Absorption (% weight increase)  0.05 - 0.5  after 24 hrs D570
Dielectric Strength (V/mil);
1/8" thick specimen unless noted
  350 - 450   D149

 Processing Properties Conditions
Type ASTM
Melting Temperature (ºC)  thermoset  Tm, crystalline  
Processing Temperature (ºC)  160 - 183  transfer molding  
 133 - 177  compression molding  
 138 - 199  injection molding  
 160 - 183  transfer molding  
Molding Pressure (MPa)   14 - 138    
Compression Ratio  1.8 - 2.5    
Linear Mold Shrinkage (cm/cm)  0.003 - 0.01   D955

Top of Page

Suppliers
Cytec Fiberite, Inc. Tempe, AZ   
Plastics Engineering, Inc. Auburn Hills, MI   
Premix, Inc. North Kingsville, OH   

Top of Page

Home  Membership  About Us  Privacy  Disclaimer  Contact  Advertise

Copyright © 2009 eFunda, Inc.