eFunda Polymers: Properties of Polyphenylene Oxide (modified) {alloy with nylon, unreinforced}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Polyphenylene Oxide (modified)
 
List of Suppliers
Additives: alloy with nylon, unreinforced
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Flexural Modulus (MPa)   2001 - 2174   23 ºC   D790
Tensile Strength (MPa)   59 at break   D638
Flexural Strength (MPa)
at yield or break
  3     D790
Elongation at break (%)   60     D638
Izod Impact (J/cm of notch)
1/8" thick specimen unless noted
  2.0     D256A

 Thermal Properties Conditions
Pressure State ASTM
Deflection Temperature (ºC)  177   0.46 MPa   D648
 122   1.82 MPa   D648

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  1.1   D792
Water Absorption (% weight increase)  1  saturated D570
 0.3  after 24 hrs D570

 Processing Properties Conditions
Type ASTM
Linear Mold Shrinkage (cm/cm)  0.013 - 0.016   D955

Top of Page

Suppliers
Ashley Polymers Brooklyn, NY   
GE Plastics Pittsfield, MA  800-845-0600