eFunda Polymers: Properties of Polyphenylene Oxide (modified) {alloy with polystyrene, 15% glass fiber reinforced}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Polyphenylene Oxide (modified)
 
List of Suppliers
Additives: alloy with polystyrene, 15% glass fiber reinforced
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Flexural Modulus (MPa)   3105 - 3450   23 ºC   D790
Tensile Strength (MPa)   69 - 83 at break   D638
Elongation at break (%)   5 - 8     D638
Hardness  106 - 110  Rockwell R   D638
Izod Impact (J/cm of notch)
1/8" thick specimen unless noted
  0.6 - 0.7     D256A

 Thermal Properties Conditions
Pressure State ASTM
Deflection Temperature (ºC)  134 - 138   0.46 MPa   D648
 123 - 127   1.82 MPa   D648

 Processing Properties Conditions
Type ASTM
Melting Temperature (ºC)  100 - 125  Tg, amorphous  
Processing Temperature (ºC)  205 - 333  injection molding  
 238 - 274  extrusion  
Molding Pressure (MPa)   69 - 276    
Linear Mold Shrinkage (cm/cm)  0.002 - 0.004   D955

Top of Page

Suppliers
GE Plastics Pittsfield, MA  800-845-0600
Polymer Resources, Ltd. Farmington, CT  800-243-5176

Top of Page

Home  Membership  About Us  Privacy  Disclaimer  Contact  Advertise

Copyright © 2009 eFunda, Inc.