eFunda Polymers: Properties of Acrylic {multipolymer, molding and extrusion compounds}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Acrylic
 
List of Suppliers
State: multipolymer
Application: molding and extrusion compounds
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Elastic Modulus (MPa)   2070 - 2967  tensile   D638
Flexural Modulus (MPa)   2001 - 2760   23 ºC   D790
Tensile Strength (MPa)   38 - 57 at break   D638
Compressive Strength (MPa)
at yield or break
  52 - 80     D695
Flexural Strength (MPa)
at yield or break
  63 - 90     D790
Elongation at break (%)   5 - 28     D638
Hardness   22 - 56  Rockwell   D638
Izod Impact (J/cm of notch)
1/8" thick specimen unless noted
  0.5 - 1.3     D256A

 Thermal Properties Conditions
Pressure State ASTM
Coef of Thermal Expansion (10-6/ºC)   44 - 50     D696
Deflection Temperature (ºC)   83 - 90   1.82 MPa   D648
Thermal Conductivity (W/m-ºC)  0.222     C177

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  1.11 - 1.12   D792
Water Absorption (% weight increase)  0.3  after 24 hrs D570

 Processing Properties Conditions
Type ASTM
Melt Flow (gm/10 min)  2 - 14   D1238
Melting Temperature (ºC)   80 - 105  Tg, amorphous  
Processing Temperature (ºC)  205 - 260  injection molding  
 194 - 244  extrusion  
Molding Pressure (MPa)   35 - 138    
Linear Mold Shrinkage (cm/cm)  0.004 - 0.008   D955