Enter Gage Number


If you know the gage number and would like to find out the actual sizes in different standards, enter it here. For sizes larger than gage 1 use the following: 7/0, 6/0, 5/0, 4/0, 3/0, 2/0, 1/0
Enter Wire Size
inch

If you know the actual size and would like to find out the corresponding gage numbers in different standards, enter it here.

American Wire (Brown & Sharpe) Gage
(exact)
0.0201
Gage 24 (0.0201) Gage 23 (0.0226)

 
Steel Wire Gage (U.S.)
0.0201
Gage 26 (0.0181) Gage 25 (0.0204)

 
British Standard (Imperial) Wire Gage
0.0201
Gage 25 (0.02) Gage 24 (0.022)

 
Music (Piano) Wire Gage
0.0201
Gage 8 (0.02) Gage 9 (0.022)

 
Birmingham (Stub's Iron) Wire Gage
0.0201
Gage 25 (0.02) Gage 24 (0.022)

 
Stub's Steel Wire Gage
0.0201
Gage 75 (0.02) Gage 74 (0.022)