engineering fundamentals O-Ring Chemical Compatibility Guide
Directory | Career | News | Standards | Industrial | SpecSearch®
Design Home
O-Rings
Overview
Design Guidelines
AS 568A Std Sizes
Chemical Resistance
Calculator
Radial O-Ring Selector
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
Instructions
This page contains a guide to selecting O-ring materials based on chemical compatibility requirements.

The chemical compatibility data can be presented in one of two ways. First, you can select a specific O-ring material to view its compatible chemicals. Or second, you can select a specific chemical to view all its compatible O-ring materials.

Chemical compatibilities are rated and displayed according to the following scale:

  Key to O-Ring Material Compatibility Ratings  
 (4)   Good, both for static and dynamic seals
 (3)   Fair, usually OK for static seals
 (2)   Sometimes OK for static seals; not OK for dynamic seals
 (1)   Poor
 (0)   No Data
 
O-Ring Compatibilities
O-Ring Materials
(select a material to show its compatible chemicals)
Aflas Buna-N (Nitrile) Butyl
Chemraz Epichlorohydrin Ethylene-Propylene
Fluorocarbon Fluorosilicone Hypalon
Kalrez Natural Rubber Neoprene
Nitrile, Hydrogenated Polyacrylate Polysulfide
Polyurethane, Cast Polyurethane, Millable Silicone
Styrene Butadiene Teflon, Virgin Vamac
 
Order by Chemical Name
Chemicals Compatible with Polyacrylate
(select a chemical to show its compatible O-ring materials)
Air below 200 C (4) Aluminium Chloride (4) Ammonium Chloride (4)
Animal Oil (4) ASTM Fuel A (4) ASTM Oil One (4)
ASTM Oil Three (4) ASTM Oil Two (4) Automatic Transmission Fluid (4)
Benzine (Ligroin) (4) Bunker Oil (4) Butane (4)
Butter (4) Calcium Chloride (4) Calcium Nitrate (4)
Carbonic Acid (4) Castor Oil (4) China Wood Oil, Tung Oil (4)
Cod Liver Oil (4) Corn Oil (4) Creosote, Coal Tar (4)
Crude Oil (Asphalt Base) (4) Dow Corning 550 (4) Elco 28 Lubricant (4)
Ethane (4) Freon 113 (4) FREON R134A (4)
Fuel Oil (4) Grease, Petroleum Base (4) Helium (4)
Heptane (4) Hexane (4) Iso Octane (4)
Lard, Animal Fat (4) Linsed Oil (4) Lubricating Oils, Petroleum Base (4)
MIL-F-25558 (RJ-1) (4) MIL-R-25576 (RP-1) (4) MIL-S-3136, Type 1 Fuel (4)
MIL-S-81087 (4) Mineral Oils (4) Neatsfoot Oil (4)
Nitrogen, Gas (4) N-Pentane (4) Peanut Oil (4)
Pine Oil (4) Potassium Nitrate (4) Potassium Sulfate (4)
Pyranol, Transformer Oil (4) RJ-1 (MIL-F-25558) (4) RP-1 (MIL-R-25576) (4)
Silicone Grease (4) Silicone Oils (4) Silver Nitrate (4)
Sodium Chloride (4) Soyabean Oil (4) Stoddard Solvent (4)
Transmission Fluid, Type A (4) Ammonium Nitrate (3) Argon (3)
ASTM Oil Four (3) Borax Solutions (3) Cyclohexane (3)
Diesel Oil (3) Di-ester Lubricant MIL-L-7808 (3) Ethyl Acetoacetate (3)
Ethylene (3) Freon 22 (3) Hydrogen Gas (3)
JP 3 MIL-J5624 (3) JP 6 MIL-J5624 (3) Methane (3)
Methanol (3) MIL-F-25656 (3) MIL-G-25760 (3)
MIL-H-5606 (3) MIL-J 5624, JP-3, JP-4, JP-5 (3) MIL-L-25681 (3)
Naphtha (3) Natural Gas (3) Oleic Acid (3)
Oxygen, Cold (3) Ozone (3) Petroleum Oil (3)
Producer Gas (3) Rapeseed Oil (3) Red Oil (3)
Turbine Oil (3) Turpentine (3) Dow Guard (2)
Ethyl Chloride (2) Isopropyl Ether (2) Methyl Bromide (2)
Phosphoric Acid (2) Radiation (2) Acetaldehyde (1)
Acetamide (1) Acetic Acid, Glacial (1) Acetic Anhydride (1)
Acetophenone (1) Acetyl Chloride (1) Acrylonitrile (1)
Alkazene (1) Aluminium Acetate (1) Aluminium Sulfate (1)
Ammonia, Anhydrous (1) Ammonia, Gas, Cold (1) Ammonia, Gas, Hot (1)
Ammonium Hydroxide, Concentrated (1) Ammonium Persulfate Solution (1) Ammonium Sulfate (1)
Amyl Acetate (1) Amyl Alcohol (1) Amyl Chloronaphthalene (1)
Aniline (1) Aniline Oil (1) Arachlor 1248 (1)
Askarel Transformer Oil (1) ASTM Fuel B (1) ASTM Fuel C (1)
ASTM Fuel D (1) Beer (1) Benzaldehyde (1)
Benzene (1) Benzene Sulfonic Acid (1) Benzoic Acid (1)
Benzophenone (1) Benzyl Alcohol (1) Benzyl Benzoate (1)
Benzyl Chloride (1) Bleach Liquor (1) Boric Acid (1)
Brake Fluid (1) Bromine Gas (1) Bromobenzene (1)
Butadiene Monomer (1) Butyl Alcohol (1) Butyl Carbitol (1)
Butyl Cellosolve (1) Butyraldehyde (1) Calcium Carbonate (1)
Calcium Hydroxide (1) Calcium Hypochlorite (1) Calcium Sulfide (1)
Carbitol 2 (1) Carbolic Acid (Phenol) (1) Carbon Disulfide (1)
Carbon Tetrachloride (1) Cellosolve (1) Chloracetic Acid (1)
Chlorinated Solvents (1) Chlorine Dioxide (1) Chlorine Trifluoride (1)
Chlorine, Dry (1) Chlorine, Wet (1) Chloroform (1)
Chlorosulfonic Acid (1) Chrome Plating Solution (1) Chromic Acid (1)
Coffee (1) Coolanol Monsanto (1) Creosylic Acid (1)
Denatured Alcohol (1) Diacetone (1) Diacetone Alcohol (1)
Dibutyl Phthalate (1) Dichloro-Butane (1) Diethylamine (1)
Diethylamine Glycol (1) Dimethyl Formamide (1) Dimethyl Phthalate (1)
Dioxane (1) Diphenyl (1) Dowtherm A (1)
Ethanol (1) Ethyl Alcohol (1) Ethyl Benzene (1)
Ethyl Benzoate (1) Ethyl Cellulose (1) Ethyl Chlorocarbonate (1)
Ethyl Diamine (1) Ethyl Ether (1) Ethyl Hexanol (1)
Ethyl Oxalate (1) Ethyl Pentachlorobenzene (1) Ethylene Dichloride (1)
Ethylene Glycol (1) Ethylene Oxide (1) Ethylene Trichloride (1)
Furan (1) Furfural (1) Furfuryl Alcohol (1)
Gallic Acid (1) Gasoline, Automotive (1) Gelatine (1)
Glycerin (1) Glycol, General (1) Hexyl Alcohol (1)
Hydrobromic Acid, Gas (1) Hydrochloric Acid (1) Hydrocyanic Acid (1)
Hydrofluoric Acid (1) Hydroquinone (1) Isobutyl Alcohol (1)
Isopropanol (1) Isopropyl Acetate (1) Isopropyl Chloride (1)
Lacquer Solvents (1) Lacquers (1) Lindol, Hydraulic Fluid (Phosphate Ester Type) (1)
Lye (1) Maleic Acid (1) Methyl Acrylate (1)
Methyl Butyl Ketone (1) Methyl Cellosolve (1) Methyl Chloride (1)
Methyl Ether (1) Methyl Ethyl Ketone (MEK) (1) Methyl Isobutyl Ketone (MIBK) (1)
Methyl Methacrylate (1) Methylene Chloride (1) MIL-H-7083 (1)
Milk (1) Monovinyl Acetate (1) Nitric Acid (1)
Nitrobenzene (1) Nitroethane (1) Nitrogen Tetroxide (1)
Nitromethane (1) Nitropropane (1) N-Octane (1)
Oleum (Fuming Sulfuric Acid) (1) Oxygen, 200-400F (1) Phenol (1)
Phenylhydrazine (1) Phosphoric Trichloride (1) Propanol (1)
Propyl Acetate (1) Propyl Alcohol (1) Propylene (1)
Propylene Oxide (1) Pydraul, 10E (1) Pydraul, 230C, 312F, 540C (1)
Pydraul, 30E, 50E, 65E, 90E (1) Pyrogard 42, 43, 53, 55 (Phosphate Ester) (1) Skydrol 500 (1)
Sodium Bicarbonate (1) Sodium Carbonate (1) Stearic Acid (1)
Styrene Monomer (1) Sucrose Solutions (1) Sulfur Chloride (1)
Sulfur Dioxide Gas, Dry (1) Sulfur Dioxide Gas, Wet (1) Sulfur Dioxide, Liquefied Under Pressure (1)
Sulfur Hexafluoride (1) Sulfur Trioxide (1) Sulfurous Acid (1)
Tannic Acid (1) Tertiary Butyl Alcohol (1) Tertiary Butyl Mercaptan (1)
Tetrabromoethane (1) Tetrachloroethane (1) Tetrachloroethylene (1)
Tetrahydrofuran (1) Tetralin (1) Toluene (1)
Triethanolamine (1) Varnish (1) Vinegar (1)
Wagner 21B Brake Fluid (1) Water, Fresh (1) Whiskey (1)
Xylene (1) Acetone (0) Acetylene Gas (0)
Aluminium Flouride (0) Aluminium Nitrate (0) Ammonium Carbonate (0)
Ammonium Phosphate (0) Amyl Borate (0) Aromatic Fuel 50% (0)
Automotive Brake Fluid (0) Carbon Monoxide (0) Chlordane (0)
Citric Acid (0) Dibenzyl Ether (0) Epoxy Resins (0)
Ethyl Formate (0) Ethyl Mercaptan (0) Ethyl Silicate (0)
Formaldehyde (0) Freon 11 (M) (0) Freon 112 (0)
Freon 114 (0) Freon 114B2 (0) Freon 12 (0)
Freon 13 (0) Freon 21 (0) Freon 31 (0)
Freon 32 (0) Freon 502 (F22+F316) (0) Freon C318 (0)
Freon TF (0) Glucose (0) Hydraulic Oil, Petroleum Base (0)
Hydrazine (0) Hydrobromic Acid (0) Hydrogen Peroxide (0)
Iodine (0) JP 4 MIL-J5624 (0) JP 5 MIL-J5624 (0)
Kerosene (0) Linoleic Acid (0) Liquefied Petroleum Gas (LPG) (0)
Malathion (0) Mercuric Chloride (0) Mercury (0)
Methyl Acetate (0) Methyl Alcohol (0) Methyl Mercaptan (0)
Methyl Oleate (0) Methyl Propyl Salicylate (0) Methylacrylic Acid (0)
Naphthalene (0) Naphthalenic (0) N-Hexaldehyde (0)
Octyl Alcohol (0) Oronite 8200 (0) Oxalic Acid (0)
Propane (0) Sea Water (0) Sodium Hydroxide (0)
Steam to 350F (0) Sulfuric Acid (Concentrated) (0) Tartaric Acid (0)
Tetrabutyl Titanate (0) Tetraethyl Lead (0) VV-H-910 (0)
White Pine Tar (0)