A J Marshall (Special Steels) Ltd are steel stockholders of abrasion resistant, high strength, CORTEN weather resistant and work hardening manganese steel plates, sheets and profiles.

 

Stocked steel grades: RAEX 400, RAEX 500, XAR300, XAR400, XAR500,  BRINAR 400, AR400, S690QL/QL1, Optim 700 MC, Dillimax 690, CORTEN weather resistant and 12-14% Manganese work-hardening steel.

 

When dealing with abrasion resistant, high strength, weather resistant and work hardening steels you cannot afford to take chances, it pays to trust a specialist.  For over thirty five years A J Marshall has supplied high quality plates, sheets and profiles to customers both throughout the UK and worldwide.

 

With the UK's largest quenched and tempered steel plate size range, 3mm-200mm thick, 99% of all enquiries can be covered from stock.  A choice of full plates, cut to length part plates or profiles. Also available if required - drilling, machining and bending services, so finished products such as bucket lips, crusher spares and dump truck reliner kits can be delivered straight to site.

 

We have the technical back up of some of the World's largest mills, so we can find an effective solution to even the most exceptional and complicated applications.

 

All steel is supplied with full mill test certificates to DIN EN 10204-3.1.

 

Delivery within 48 hours (Britain), within 72 hours (Ireland) and exports worldwide direct from ourselves.

 

Products

Steel plates, steel sheets and steel profiles.

 

Abrasion Resistant Steel Wear Plate:

RAEX 400, RAEX 500, XAR-300, XAR-400, XAR-500, BRINAR 400, AR400, 20Mn Cr6-5.

 

High Strength Structural Steel Plate: 

S690QL, S690QL1, Optim 700 MC, STRENX, 700MCD, Dillimax 690, RQT 701, Supralsim 690, Maxil 690, S700MC.

 

Weather Resistant Steel Plate: 

CORTEN, COR-TEN A, COR-TEN B, PATINAX, S355J2WP+N, S355J2W+N, S355JOWP, S355JOW, S355J2W.

 

Work Hardening Manganese Wear Resistant Steel Plate: 

12/14% Manganese, X120 Mn12, X120 Mn13, Creusabro M, ASTM A128 Grade B2, DIN W1.3401.

 

Also available if required - drilling, machining, bending and testing services.

Address Unit 89 Marston Moor Business Park
Rudgate
Tockwith
York
North Yorkshire
YO26 7QF
Country United Kingdom
Telephone +44 01423 359111
Fax +44 01423 359222
Email jo-anne.hardy@ajmarshall.com
Website www.ajmarshall.com
 Showcase Products
 

click image to enlarge.
ABRASION RESISTANT STEEL WEAR PLATE

Stocked steel grades: RAEX 400, RAEX 500, XAR300, XAR400, XAR500, BRINAR 400, AR400, 20MnCr6-5.

 

RAEX 400

360-440HB

3mm - 100mm+

RAEX 500

450-540HB

6mm - 50mm

XAR300

270–340HB

      10mm - 50mm

XAR400

360-440HB

      3mm - 120mm+

XAR500

450-530HB

      6mm - 50mm

                                               

RAEX STEELS

RAEX is a hot rolled hardened steel grade with excellent hardness and strength properties and is resistant to abrasion and extreme surface pressure.  RAEX 400 extends the lifespan of machinery, decreases the impacts of wear in structural components and saves costs.  Thanks to its high strength properties, RAEX allows innovative and environmentally sound product development.  RAEX is easy to weld, cut and has reasonably good formability.

 

TYPICAL APPLICATIONS:  Buckets and cutting edges of earth-moving machines, wearing parts of mining machines, wearing parts of concrete mixing plants and wood processing machines, platform structures, feeders and funnels.

 

XAR STEELS

XAR wear resistant special structural steels may be used for wear-exposed structures, e.g. excavating, mining and earth-moving machinery, excavator buckets, truck dump bodies, dredgers, conveying, crushing and pulverizing equipment, scrap presses and paving moulds.

 

All steel is supplied with full mill test certificates to DIN EN 10204-3.1.

 

Payment:  L/C, T/T, Cheque, Transfer, Cash, VISA.

 

 

-Materials, Chemicals and Adhesives > Metals and Alloys
 

click image to enlarge.
HIGH STRENGTH STRUCTURAL STEEL PLATE

Stocked steel grades:              S690QL, S690QL1, Optim 700 MC, STRENX, 700MCD, S700MC, Dillimax 690, RQT, Supralsim 690, Maxil 690.

 

S690 QL/QL1

6mm-200mm

690 N/mm2 guaranteed min yield.

Optim 700 MC

3mm-5mm

700 N/mm2 guaranteed min yield.

 

S690 STEELS

S690 steel is a high strength quenched and tempered fine-grain structural steel.  Dedicated for structure and enables to make weight savings thanks to a minimum yield strength of 690 N/mm2.

 

TYPICAL APPLICATIONS:  Heavy road vehicles: chassis, dumper bodies.  Cranes construction: booms of mobile cranes.  Structural steelworks: bridges, bridge components, components for offshore structures.  Pressure vessels: fixed and transportable storage tanks, vessels.  Power plants: penstocks, spiral cases.  Materials handling: lifting and mobile equipment.  Mining and earthmoving equipment: roof supports etc.  Agricultural equipment and trailers.

 

OPTIM 700 MC STEELS

Optim MC is a thermo-mechanically rolled steel, offering both strength and formability.  It makes equipment manufacturing more efficient thanks to good weldability, flangeability and lower unit weight.  The properties promote environmentally friendly construction and sustainable development.  Steel structures can be made lighter, which means that the payload of machines and equipment can be increased and fuel consumption reduced. 

 

TYPICAL APPLICATIONS:  Heavy road vehicles: chassis, dumper bodies.  Cranes construction: booms of mobile cranes, forestry vehicles, crane arms and other lifting equipment.  Structural steelworks: bridge components, components for offshore structures.  Pressure vessels: fixed and transportable storage tanks, vessels.  Power plants: penstocks, spiral cases.  Mining equipment: roof supports.  Load handling equipment and masts.

 

All steel is supplied with full mill test certificates to DIN EN 10204-3.1.

 

Payment:  L/C, T/T, Cheque, Transfer, Cash, VISA.

-Materials, Chemicals and Adhesives > Metals and Alloys
 

click image to enlarge.
WEATHER RESISTANT STRUCTURAL STEEL PLATE

Stocked steel grades:  CORTEN, COR-TEN A, COR-TEN B, PATINAX, S355J2WP+N, S355J2W+N, S355JOWP, S355JOW, S355J2W, 1.8946, 1.8965.

           

1.5mm-50mm

345-355 HB

 

COR-TEN/CORTEN STEELS

Weather resistant structural steel.  The anticorrosive properties of weather resistant steel are better than those of other structural steels in many applications.  The steel is self-protecting:  the rust layer on the surface becomes a tight oxide layer that slows down the progress of corrosion.  The steel is an economical, long-lasting and fully recyclable material.

 

TYPICAL APPLICATIONS: The steel is used for various types of welded, bolted and riveted constructions e.g. steel frame structures, building cladding, metal sculptures (Angel of the North), chimneys, bridges, tanks and containers, exhaust systems, vehicles and equipment constructions.

 

All steel is supplied with full mill test certificates to DIN EN 10204-3.1.

 

Payment:  L/C, T/T, Cheque, Transfer, Cash, VISA.

-Materials, Chemicals and Adhesives > Metals and Alloys
 

click image to enlarge.
WORK HARDENING MANGANESE WEAR RESISTANT STEEL PLATE

Stocked steel grades:  12/14% Manganese, X120 Mn12, X120 Mn13, Creusabro M, ASTM A128 Grade B2, DIN W1.3401.

           

6mm-12mm +

360-440 HB

 

MANGANESE STEELS

A high manganese, fully austenitic, quench annealed, non-magnetic, work hardening steel with an exceptionally high level of wear resistance when subjected to work hardening by shock or high impact pressure in service.  Severe wear on the surface has a work-hardening effect on the austenitic structure of this steel.  This, when combined with the level of carbon in accordance with the international standards, leads to an increase in hardness from 200BHN (in as delivered plates) up to an in-service hardness of at least 600BHN.  This work-hardening capability renews itself through out in-service life.  The underlayers not work-hardened maintain an excellent resistance to shock and a very high ductility.

 

TYPICAL APPLICATIONS:  Quarries and Constructions:  Earth moving crusher jaw, grizzly, screen, stone chutes, chain guide and shredder plates, shovel buckets.  Mines:  Bucket blade of loader, chain conveyor parts, sprocket wheel, various armouring elements.  Iron Industry, Foundry:  Guiding and shifting plates, scraps container, liner of shot blasting unit, pedestal liner, flanged bolster cup, wear liner.  Concrete and Brickworks:  Core and dividing wall of parpen mould, grinding mill scraper, mixer paddle.  Scraps - Recoveries:  Wheel disk, striker and hammer mill.  Automotive Industries:  Shot blasting equipment.

 

All steel is supplied with full mill test certificates to DIN EN 10204-3.1.

 

Payment:  L/C, T/T, Cheque, Transfer, Cash, VISA.

-Materials, Chemicals and Adhesives > Metals and Alloys
 
 

Related Product Categories
Materials, Chemicals and Adhesives
Metals and Alloys
Any of various opaque, fusible, ductile, and typically lustrous substances that are good conductors of electricity and heat, form cations by loss of electrons, and yield basic oxides and hydroxides.
 
  Home  About Us  Privacy  Disclaimer  Contact  Advertise