Hi everyone,

Can anyone please tell me what machinable pre-hard steel has the
highest compressive yield strength ? I'm guessing it would be a pre-
hard 4000 series, perhaps 4340 or a bearing steel or pre-hard tool
steel.

I'm looking for the highest yield strength I can find in a steel that
is still machinable, i.e., not so hard that it can't really be
machined effectively. Depending on how the part is machined, I would
need a thickness of around 1.338" or 1.585".

Thanks
John
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (3)
8620 is widely used in the bearing industry and often machined preheat trea...
No. 19885, Posted by dr6mm on 07/14/08, 10:26 PST.
A little more information would be helpful.  EDM (electric discharge m...
No. 19880, Posted by gbynum on 07/11/08, 19:19 PST.
Can I ask what is the application ?Machinable  with what machine?What ...
No. 19793, Posted by devitg on 06/01/08, 07:50 PST.