I have to determine the temperature and time required to anneal C26000 brass and C11000 copper.  I am looking for some general guidelines to use.
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (1)
Hi there, The annealing temperatures for cold-worked coppers are well de...
No. 23, Posted by dr funda on 01/07/00, 09:17 PST.