Message No. 22736, Started by bluepiece on 08/23/18

Good day everyone, 

I have a question regarding the terminology of cold working and work hardening. I read somewhere that they are synoymous, but are they really? To my knowledge, cold working refers to the plastic deformation of metal parts at low temperatures. As far as I know, cold working is not deliberatr while work hardening is. Am I wrong??

Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (18)
I think your article mentioned a certain aspect of the problem. I think it ...
No. 23469, Posted by JenniferRogers on 06/13/19, 01:18 PST.
I think your article mentioned a certain aspect of the problem. I think it ...
No. 23468, Posted by JenniferRogers on 06/13/19, 01:16 PST.
Thank for your writting. You have made it very clear that the problem is ha...
No. 23184, Posted by alanabui on 04/23/19, 00:26 PST.
Thank you for sharing valuable information cat mario  
No. 23120, Posted by lindarose11 on 04/18/19, 00:33 PST.
great article, I was very impressed about it, wish you would have stayed ne...
No. 23117, Posted by phamyen on 04/17/19, 20:06 PST.
Very helpful advice in this particular post! It’s the little changes ...
No. 23114, Posted by alicetaylor on 04/17/19, 19:52 PST.
Hello, just wanted to say, I loved this article. It was practical.   ...
No. 22891, Posted by alicetaylor on 02/26/19, 19:58 PST.
Hotmail is free webmail service provided by Microsoft, basically this email...
No. 22863, Posted by abrahamlincoln on 02/20/19, 23:15 PST.
 Oh! This article has suggested to me many new ideas. I will embark on...
No. 22842, Posted by funnyjokes on 01/18/19, 01:24 PST.
Hello, just wanted to say, I loved this article. It was practical.   ...
No. 22838, Posted by alicetaylor on 01/16/19, 20:45 PST.
hmmm, this is a nice question hah, But I think it is more different than yo...
No. 22835, Posted by garen123 on 01/11/19, 07:17 PST.
This is also a very good post which I really enjoyed reading. It is not eve...
No. 22802, Posted by lindarose11 on 12/25/18, 23:25 PST.
Work hardening, also known as strain hardening, is the strengthening o...
No. 22799, Posted by pri2347 on 12/21/18, 23:38 PST.
These words are synonyms. See how to differentiate similar words at ht...
No. 22797, Posted by amyneild on 12/20/18, 12:06 PST.
i think so, run 3 full game
No. 22768, Posted by vermaruby38 on 11/11/18, 23:58 PST.
I have never consider this two terms as synonims. Even google says the are ...
No. 22761, Posted by stepforward on 10/19/18, 12:53 PST.
You’ve helped make it clearer for me! run 3
No. 22754, Posted by rosabella on 10/09/18, 02:00 PST.
Hi Bluepiece-  I've used "cold working" and "work hardening" as near s...
No. 22739, Posted by gearloose on 08/28/18, 19:39 PST.