I have a requirement for

 

 

CASE HARDEN USING CARBONITRIDING TO .007 - .015 TOTAL CASE

DEPTH TO R15-N 83-88.

I understand the .007-.015 total case depth element, but I think I am not understanding what the 83-88 value represents. Is there someone familiar with this who can explain in simple terms what the requirement is here?

 

 

Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (2)
This is very useful information for me. Thank you very much! Look rese...
No. 23132, Posted by CarlaCoach on 04/19/19, 10:50 PST.
The 83-88 is a reading on the R15N (Rockwell) scale.  Thin case harden...