Message No. 64, Started by APOORV on 01/18/00
WOULD LIKE TO KNOW THE NAME OF MANUFACTURES OF CARBON STOPOFF PASTE USED IN CASE CARBURISING PROCESS OF HEAT TREATMENT
                 ON APPLICATION OF CARBON STOPOFF TO THE SURFACE OF PRODUCT TO BE CASE CARBURISED THE CARBON PENETRATION DURING THE DIFFUSION CYCLE OF GAS CARBURISING DOES NOT TAKE PLACE THEREBY MANTAINING SELECTIVE CASE HARDENING .
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (11)
Dear Mr. Apoorv, While going thro' your old e-mail in efunda, I came a...
No. 18851, Posted by eskayshah on 06/13/07, 06:03 PST.
Dear Sir,We would like tell all the details about our company details later...
No. 17290, Posted by samantula on 02/10/06, 07:33 PST.
hey, no problem, I'm used to the taste of shoe leather myself.... Haven'...
No. 10940, Posted by rorschach on 04/02/03, 15:01 PST.
Rorschach, the reason for the discrepancy is my typing before thinking in t...
No. 10937, Posted by gearloose on 04/02/03, 14:25 PST.
Gearloose, I respect your knowledge in this matter, however this does not j...
No. 10931, Posted by rorschach on 04/01/03, 13:17 PST.
While it's not a "stop-off" in the paint-it-on sense of the phrase, copper ...
No. 10930, Posted by gearloose on 04/01/03, 06:18 PST.
liquid nitriding is a whole other animal, to my knowledge, there are no sto...
No. 10918, Posted by rorschach on 03/31/03, 08:00 PST.
I was just looking around and I know Im a bit late, but my company produces...
No. 10915, Posted by jmorris on 03/31/03, 06:45 PST.
please send to my e mail about liquid carburizing send to aang_helmy @yaho...
No. 7162, Posted by axl_helmy on 05/24/01, 04:03 PST.
Actually, a number of firms make carburizing and nitriding stop-off paints,...
No. 3082, Posted by gearloose on 07/26/00, 06:35 PST.
Out of curiosity I looked for this product you describe, and I can't find a...
No. 3069, Posted by canucme on 07/25/00, 10:38 PST.