Dear Sir,

Please inform me the Youngs Modulus for Aluminium alloy (A356.2).

Thanking you,

Sincerely,

Raju
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (2)
Hello Raju! A356, a 7% Si, 0.3% Mg cast aluminum alloy, has a Young's modu...
No. 6504, Posted by gearloose on 03/21/01, 06:18 PST.
Never heard of your aluminium spec A356.2, do you have a US or UK equivalen...
No. 6502, Posted by neil moran on 03/21/01, 01:29 PST.