in diesiel engines running on Heavy fuel oil why the Exhaust valves used to fail due to stem corrosion.
What is exactly is the stem corrosion and what is its reasons?


versh
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (2)
Stem corrosion, and corrosion in general, can be reduced by using alloy 20 ...
No. 21909, Posted by pfeinstein on 11/16/12, 14:46 PST.
Heavy fuel oil used may contain sulphur. burnt sulphur may condense and cor...
No. 914, Posted by processtrade on 03/28/00, 19:18 PST.