Message No. 9257, Started by devitg on 05/24/02
Please help me :

I need to know what kind  of steel is a

DC04

under the french norm NF EN 10 130.

a equivalent to aisi or sae will be the best, if not the composition.

It seem to be some near SAE 1010 .

It is used to do rivets.

Thanks

Gabriel

k281969@hotmail.com

Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (2)
Hi Gearloose: Thanks for it. Gabriel
No. 9273, Posted by devitg on 05/28/02, 14:10 PST.
Hi Gabriel! I don't have the EN specifications, but according to my Stah...
No. 9271, Posted by gearloose on 05/28/02, 11:35 PST.