Can anyone point to a material that is non conductive and  will operate at temperatures above approx 270 ~ 280 degrees celcius.
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (15)
Kapton by Dupont is a wonderful high temp plastic. It is used for flex cir...
No. 11520, Posted by thoughttrain on 06/30/03, 12:46 PST.
by the way, he e-mailed me, his profile doesn't have an e-mail address atta...
No. 11236, Posted by rorschach on 05/18/03, 21:20 PST.
I know art, never said it did, I was just trying to fill in blanks that he ...
No. 11235, Posted by rorschach on 05/18/03, 21:18 PST.
The thread never mentioned most of these other things and I never e-mailed ...
No. 11227, Posted by art2000 on 05/16/03, 19:32 PST.
from my conversations via e-mail and his previous post concerning ESD safe ...
No. 11224, Posted by rorschach on 05/16/03, 10:12 PST.
ESD was never discussed as a problem. I interpreted the original problem as...
No. 11217, Posted by art2000 on 05/15/03, 21:18 PST.
Art, use of an isolation transformer is a definite no-no in ESD situations,...
No. 11211, Posted by rorschach on 05/15/03, 06:31 PST.
You really make it very difficult for one to provide you with help with the...
No. 11210, Posted by art2000 on 05/14/03, 22:20 PST.
Thought of Porcelin or HDPE. But it all will depend on application where th...
No. 11184, Posted by smog on 05/12/03, 04:58 PST.
maybe you can use TEFLON
No. 11177, Posted by devitg on 05/10/03, 09:21 PST.
I agree, FR4 (another good possibility as it is flame retardant as well) ci...
No. 11169, Posted by rorschach on 05/09/03, 10:20 PST.
Just because the soldering iron is at 270-280 degrees doe'nt mean that the ...
No. 11166, Posted by spike78 on 05/08/03, 15:31 PST.
What about phenolic (especially linnen based phenolic, which has a higher ...
No. 11160, Posted by rorschach on 05/08/03, 10:17 PST.
Hi, This is only used on small fixture, the only requirements that it wo...
No. 11158, Posted by noelkelly36 on 05/08/03, 09:18 PST.
according to the Freie Universitaet Berlin, 280.00 degC = 536.00 degF n...
No. 11157, Posted by gerdb on 05/08/03, 09:08 PST.