Message No. 116, Started by quiche on 01/24/00
Where can I find the thermal expansion coefficient for a particular steel alloy?  I am interested in the 300 series stainless steels, specifically 304, 316 and 316L.
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (3)
ASME B31.1-1989 has proven to be a good reference for both the mean and lin...
No. 124, Posted by hummer on 01/26/00, 04:50 PST.
A note on 316L, we couldn't find any information in our sources or with a q...
No. 120, Posted by dr funda on 01/24/00, 19:42 PST.
I found the answers to your 2 of your questions right here on eFunda under ...
No. 119, Posted by daffodil on 01/24/00, 19:02 PST.