in simple terms what are the effects of various alloying elements on aluminium alloys with respect to end use?and  which elements are detrimental and in what way and to what extent?
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (1)
There is a discussion on this in die-casting of the process section. Ple...