I am looking for Piezo-electric materials with large strain / voltage ratio (I hope this is the correct terminology), which would allow us to move an optical element with reasonable voltage.

Can you please help me where I can find a handy table with the known piezo-electric elements and their properties.

Thanks,

Mik
Reply | Start a New Topic | List Recent Topics
 

Follow-up Messages (1)
Hi, Try looking at one of the PZT-5 materials, such as PZT-5A or PZT-5H....