Hi

 

I have a question about annealing oprocedure of gold foils (BAu-4).

I have bought some foils with no annealing condtion and right now I have to do it.

 

Please help me about right procedure.

Heat treatment temperature, time, heating rate , cooling rate, colling media , furnace atmosphere and so on.

 

Thanks