| Composite Materials |
|
|
GRE consists of glass fibers in an epoxy matrtix
GRP consists of... |
|
| stress concetration factor (SCF) |
|
|
The relation is
K = 1 + q(Kt-1) ... |
|
| PIN ENGAGEMENT |
|
|
Does anyone know of the required pin engagement depth for a steel... |
|
| How much force to bend 3mm x 15mm 80,000psi steel. |
|
|
You need to klnow the length to determine this and even then at 9... |
|
| Moment of Inertia |
|
|
Yes, it is.
In your case I(a) is inertia of C section an... |
|
You need to calculate the inertia of the plate and inertia of the... |
|
| mechanical resonance mechanical spring mass forced by |
|
|
Not sure of your question - is not the answer the same as your qu... |
|
| Danger in using full threaded screw in place of partial thread? |
|
|
Are these screws that go thru a clearance hole and then&nbs... |
|
| Thread Dimensioning |
|
|
The thread length per NAS standards is measured to the bottom of ... |
|
| I beam Rating |
|
|
That sounds about right. For a simple support beam 25 feet ... |
|
| Stress relieving of aluminum weld mount |
|
|
Typical stress relief is done between 200F and 400F. If you... |
|
Question: If the part was warped after welding and you went to 20... |
|
Stress relief requires both time and temperature so maybe it was ... |
|
After welding 6061-T6, temper will drop to T4 within one inch of ... |
|
| Tensile strength |
|
|
Tensile strength is measured by a tensile testing machine with&nb... |
|
| natural frequency |
|
|
For a single degree of freedom, frequency is 3.13/sqrt deflection... |
|
The equation you mention is close( 3.13/sqrt deflection) - i... |
|
| Material Properties |
|
|
You can get technical data ( strength, etc.) from www.matweb.com.... |
|
| Bolt load difference between col and hot |
|
|
Sure, it is rather straightforward.
It can be simplified by assu... |
|
| M3 x 0.5 Nut internal diameters? |
|
|
According to the Machinery's handbook, the minor diameter externa... |
|
| Window for pressurized chamber made from laminated glass? |
|
|
No problem, happy to respond any time.
Glass is VERY strong with... |
|
it would take moree space than these boards can print to ... |
|
Usually our windows are circular not rectangular. And we opearte ... |
|
Under 2 atm pressure (30 psi) I calcualte a stress of 2700 psi fo... |
|
| Steel Mechanical properties. |
|
|
I believe that would be in the process of manufacturing the ... |
|
| Beam Stress |
|
|
You need to supply the length of the beam and then the calculatio... |
|
| What is membrane stress? |
|
|
Membrane stress is the tensile stress developed in the vessel.&nb... |
|
| tapered beam deflection |
|
|
I agree, this is a difficult solution because the inertia is vary... |
|
| Properties of steels at high temperature |
|
|
MIL HDBK 5 has properties up to 800C and stress train diagrams up... |
|
| Formula for calculating the pull-out force of a screw from wood |
|
|
Yes, sure, this is standard strength of materials theory. I... |
|
|
|
|