aluminum vs. steel in brake disc
You are completely correct, good points. The ceramic coated Ti r...
Posted 07/08/03 12:37 PST
Are there standard slurrys for wear testing?
I am looking to build a wear testing machine. I want to try to du...
Posted 07/06/03 09:09 PST
Ultimate load capabilities of M10 x 1.5 bolt
Thanks again! -Paul
Posted 07/06/03 08:59 PST
aluminum vs. steel in brake disc
Deconti Industries was a company that I worked with for MMC (Meta...
Posted 07/05/03 15:11 PST
Ultimate load capabilities of M10 x 1.5 bolt
Thank you. That helps a lot. One more question. How do you dete...
Posted 07/05/03 13:20 PST
Ultimate load capabilities of M10 x 1.5 bolt
I am looking to find the maximum shear load that can be applied t...
Posted 07/04/03 11:30 PST
aluminum vs. steel in brake disc
I have done a lot of work on designing brake rotors for mountain ...