1040 and 4340 steel
What is the difference?
Posted 03/01/00 08:28 PST
Cooling from an austenizing Temp.
samples were austenized at 850C and quenched in water, oil air an...
Posted 03/01/00 08:27 PST
Activation Energy
How is the Activation Energy for Recrystallization of copper and ...
Posted 02/21/00 09:35 PST
Annealing copper and brass
What type of process should I follow
Posted 02/13/00 14:29 PST
Rolling copper and Brass
I am involved in a lab experiment where I rolled copper and 70/30...