engineering fundamentals Member Info (samingale)
Directory | Career | News | Standards | Industrial | SpecSearch®
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
 
  

Posts by samingale
[ Order by Time Posted ] [ Group by Topic ] [ Topics by samingale ] [ All Topics ]
How to measure dB of Head Phone?
How to measure dB of Head Phone?
Posted 10/25/04 20:32 PST
What is Fresnel Lense in OHP Beamer
What is Fresnel lense ? What is its function in OHP (Over Head Pr...
Posted 10/25/04 20:31 PST
Why loosening torque is lesser than the tightening torque for bol...
Please consider standard condition i.e. no corrosion, no imperfec...
Posted 10/22/04 20:15 PST
Why loosening torque is lesser than the tightening torque for bol...
Can anybody give me proof for : Opening or loosening torque of sc...
Posted 10/19/04 02:02 PST
Acrylic for solar water heater
Can we use Acylic sheet instead of glass in solar water heater ?
Posted 10/02/04 04:17 PST
STANDARD TOLERANCE FOR UNSPECIFIED TOLERANCE FOR ANGLE IN DRAWING
I got the answer. It is specified in Westernman's Handbook - page...
Posted 09/16/04 00:39 PST
STANDARD TOLERANCE FOR UNSPECIFIED TOLERANCE FOR ANGLE IN DRAWING
Is there any standard which defines tolerance for unspecified tol...
Posted 09/14/04 20:48 PST
FUNGUS ON BAKELITE
Dear rorschach, I can not collect infirmation about anti-fungal ...
Posted 08/16/04 20:47 PST
ANODISING FOR ALUMINUM WITH SS ACCESORY
I want to anodise the aluminium object which has SS304 bracket ri...
Posted 08/16/04 20:31 PST
FUNGUS ON BAKELITE
Thank you very much. Now I will search for the anti-fungus materi...
Posted 08/11/04 22:02 PST
RUBBER GASKET DIAMETER MEASUREMENT
How we can measure inside diameter of the nitrile rubber gasket a...
Posted 08/11/04 01:35 PST
CONDUCTIVE RUBBER
Is there any electric conductive rubber? Its conductivity should ...
Posted 08/11/04 01:33 PST
FUNGUS ON BAKELITE
We are getting fungus on bakelite handles after some months / yea...