engineering fundamentals Discussion Forum
Directory | Career | News | Standards | Industrial | SpecSearch®
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
List Recent Topics | Start a New Topic
 

<< Previous Message No. 10232 Next >>
Author: ddelaiar
Time: 12/18/02 12:34 PST
This is a reply to message no. 10230 by rolschwarz
Reply | Original Message | New Topic | List Topics | List Messages on This Topic
Current Topic:
Grinding Tungsten
well, I pretty much got it done.  A colleague has a dremel tool with a small, rough grinding plate on it.  I think its got diamonds in it, but I'm not sure.  Regardless, it seems to have done the job.  Thanks for all the help.  I'm only making a handful of these prototypes (5-10), so some of the suggestions were a bit too expensive for the quantities needed, but I appreciate the input.