Sir,
Imagine what woul happen to nodules of ductile iron at elevated temperature under stress... the nodules would break up and the matrix structite would perhaps look like FG iron making it more prone to fracture as the discontinuity in the matrix(carbon flakes) would increase.

regards

lakhtin...