Author: lakhtin
Time: 10/06/05 04:03 PST
Reply | Original Message | New Topic | List Topics | List Messages on This Topic
Current Topic:
retained austinite
Sir,
why does high carbon steel and alloy steel have retained austinite in it?
i have heard that it causes soft spots in the final structure of the steel.
also that it is very brittle.
what is austempering and martempering?


regards

lakhitn...