Hullo Sathyan,

A Google search brought me to page 34 of

http://www.jfe-steel.co.jp/en/products/sheets/catalog/b1e-001.pdf

ASTM A1011-2001 Gr 60 Cl.1 & 2 seem to relate to your 410

It may be an Indian Standard as it has IS not ISO.  I suggest you do some Google searches yourself before asking the rest of us.