HELLO ALL:  I am familiar with dye penetrant and magnetic particle crack detection, but I am asking for input/references on other, newer methods such as ultrasonic acoustic emission.  I am interested in equipment availabie, ease of use, ease of interpretation, relative costs, and the tough one is cost/benefit.  The material is 2000 series aluminum which is painted all over and with machined pockets on one side.

Your inpur will be helpful

Regards

Dave