Lead tin copper Elotroplating problem

Versh, 95% of the time I've had this problem, it was due to lack of proper cleaning of the substrate, and perhaps of the intermediate layers.  I suggest you review the steps you are using to clean the article you are trying to electroplate.

 

Good luck!

 

gearloose