Cutting Speed of a Glass Fiber Reinforced Polyester
I have a material GFRP. I want to shape it with a 6 axis robot by cutting and drilling. I made the part tested and figured the bending and tensile strengths out. I also know the proporties of the cutting tip that i have. It has 2 cutting edge and dia is 6 mm. Is there any formula or a way to decide what rpm and moving speed i should use?thank you all