dear dr. funda: material properties of beryllium copper
Hi there,

1. There are indeed a few beryllium copper alloys in eFunda's database for materials. Follow this link for more information: Go!

We are currently revising our database so expect much more data in the near future.

2. Our search does try to screen out some common spelling errors. However, that part does need to be perfected so stay tuned...

Thank you for using eFunda!