METAL HEAT TREATMENT, carbon stopoff paste for carburizing
liquid nitriding is a whole other animal, to my knowledge, there are no stop-off's that are suitable for salt bath nitriding. stop-offs are only suitable for gas nitriding/carburizing. the only "stop-off" that can be used in liquid Nitriding is simply controlling how much of the part gets immersed in the molten salt.